Evaluation on tribological characteristics of (TiC+TiB)/Ti–6Al–4V composite in the range from 25 °C to 600 °C

Wear5.00
Volume: 450-451, Pages: 203256 - 203256
Published: Jun 1, 2020
Abstract
The tribological characteristics of 6%(TiC + TiB)/Ti–6Al–4V composite against Cr12MoV steel were systematically investigated using a pin-on-disc wear machine in a static temperature range of 25–600 °C. At 25 °C, the wear rate variation was proportional to the load and inverse to sliding speed. Meanwhile, the wear mechanism underwent a transition from delamination and slight oxidative wear at 0.11 m/s to delamination and abrasive wear at 0.22 m/s...
Paper Details
Title
Evaluation on tribological characteristics of (TiC+TiB)/Ti–6Al–4V composite in the range from 25 °C to 600 °C
Published Date
Jun 1, 2020
Journal
Volume
450-451
Pages
203256 - 203256
Citation AnalysisPro
  • Scinapse’s Top 10 Citation Journals & Affiliations graph reveals the quality and authenticity of citations received by a paper.
  • Discover whether citations have been inflated due to self-citations, or if citations include institutional bias.