Treatment of Goat Femur Segmental Defects with Silica-Coated Hydroxyapatite—One-Year Follow-Up

Volume: 16, Issue: 2, Pages: 385 - 391
Published: Feb 1, 2010
Abstract
Segmental bone defects caused by tumor resections, trauma, and skeletal abnormalities such as osteomyelitis remain a major problem in orthopedics because of the lack of predictability in attaining functional bone after the treatment. The objective of this study was to propose an indigenous porous biodegradable triphasic ceramic (calcium silicate, tricalcium phosphate, and hydroxyapatite [HA])-coated HA (core) (HASi) for the repair of such...
Paper Details
Title
Treatment of Goat Femur Segmental Defects with Silica-Coated Hydroxyapatite—One-Year Follow-Up
Published Date
Feb 1, 2010
Volume
16
Issue
2
Pages
385 - 391
Citation AnalysisPro
  • Scinapse’s Top 10 Citation Journals & Affiliations graph reveals the quality and authenticity of citations received by a paper.
  • Discover whether citations have been inflated due to self-citations, or if citations include institutional bias.