Microstructure and property of Cu–2.7Ti–0.15Mg–0.1Ce–0.1Zr alloy treated with a combined aging process

Abstract
A combined aging process has been developed to improve the comprehensive properties of Cu–2.7Ti–0.15Mg–0.1Ce–0.1Zr alloy. This process involved pre-aging at an elevated temperature, cold rolling, and final aging at low temperature. The alloy treated by this process was found to have good electrical conductivity and super-high strength. As the alloy was solution treated at 850 °C for 2 h, aged at 450 °C for 8 h, then cold rolled with the...
Paper Details
Title
Microstructure and property of Cu–2.7Ti–0.15Mg–0.1Ce–0.1Zr alloy treated with a combined aging process
Published Date
Jan 1, 2016
Volume
650
Pages
345 - 353