This work presents an experimental technique developed to assess sensitivity of cracking due to the property gradients in the layers of cement-based materials used as a bonded overlay. The non-uniform moisture distribution in materials causes differential length changes as a result of the combination of shrinkage, creep and strain relaxation effects. In this study, several tests are used for the purpose of predicting the differential behaviour (hydric, hydration, porosity and strain gradients) o...
7 CitationsSource
#1A. Brahma (INSA: Intelligence and National Security Alliance)
#2J-P. Ollivier (INSA: Intelligence and National Security Alliance)H-Index: 8
Last. Ch. H. Detriche (INSA: Intelligence and National Security Alliance)H-Index: 5
view all 3 authors...
Le sable-laitier est und materiau composite constitue essentiellement d’un ou de plusierus sables, d’un laitier vitrifie et d’activant. Il est principalement utilise dans la confection des assies de chaussees. On parle de sable-laitier lorsque le materiau de base est le sable.
Source
#1Jean-Paul Balayssac (INSA: Intelligence and National Security Alliance)H-Index: 18
#2Ch. H. Detriche (INSA: Intelligence and National Security Alliance)H-Index: 5
Last. N. Diafat (INSA: Intelligence and National Security Alliance)H-Index: 2
view all 3 authors...
L’objectif de cet article est de quantifier les effets de la duree de cure humide sur les caracteristiques du beton de peau en termes d’absorption capillaire et de profondeur de carbonatation. Huit formulations de beton realisees a partir d’un ciment Portland artificiel et d’un ciment Portland avec ajouts sont etudiees afin de couvrir une grande partie du domaine d’utilisation courante du beton. Les resultats montrents que les caracteristiques du beton de peau a un an sont etroitement liees a la...
7 CitationsSource
#1Jean-Paul Balayssac (INSA: Intelligence and National Security Alliance)H-Index: 18
#2Ch. H. Detriche (INSA: Intelligence and National Security Alliance)H-Index: 5
Last. N. Diafat (INSA: Intelligence and National Security Alliance)H-Index: 2
view all 3 authors...
Si par manque d'eau, l'hydratation du liant relentit ou s'arrete, l'evolution des caracteristiques mecaniques du beton reste inachevee. Le role de la cure est de maintenir une humidite suffisante durant l'hydratation de telle sorte que les proprietes desirees soient atteintes.
9 CitationsSource
#1Jean-Paul Balayssac (INSA: Intelligence and National Security Alliance)H-Index: 18
#2Ch. H. Detriche (INSA: Intelligence and National Security Alliance)H-Index: 5
Last. J. Grandet (INSA: Intelligence and National Security Alliance)H-Index: 2
view all 3 authors...
Abstract Even if mix design (cement content, W/C ratio) has an effect on durability of concrete mixed with blended cement, curing conditions, particularly curing time, also affect concrete durability against carbonation. The choice of curing time depends on cement content, and must be adjusted to concrete design (28 day strength, W/C ratio). Concretes with a low cement content (or a high W/C ratio) must be cured longer than those having higher cement content. Finally, some correlations show that...
59 CitationsSource
#1Jean-Paul Balayssac (INSA: Intelligence and National Security Alliance)H-Index: 18
#2Ch. H. Detriche (INSA: Intelligence and National Security Alliance)H-Index: 5
Last. J. Grandet (INSA: Intelligence and National Security Alliance)H-Index: 2
view all 3 authors...
Les auteurs motivent leur choix en faveur de l'essai d'absorption d'eau pour la caracterisation de la porosite du beton d'enrobage et de la dimension de ses plus gros capillaires, facteurs essentiels vis-a-vis de la durabilite a la carbonatation. Daus ce but, ils s'appuient sur un modele existant, utilise pour des terres cuites, et ils l'etendent au materiau beton. A partir de ces elements, le critere retenu est la quantite d'eau absorbee au bout d'une heure, suffisamment repesentative du rayon ...
13 CitationsSource
#2Ch. H. DetricheH-Index: 5
Last. J Grandet
view all 3 authors...
La carbonatation est un facteur essentiel vis-a-vis de la durabilite des ouvrages en beton arme. En entrainant la depassivation des armatures, l'action du gaz carbonique risque de provoquer leur corrosion. Le temps necessaire a l'accomplissement de ce phenomene est relativement long, d'autant plus long que la porosite du beton d'enrobage est faible. Des essais de carbonatation acceleree realises en ambiance a forte teneur en CO2 fournissent des resultats exploitables au bout d'un temps relativem...
#1Francois Saucier (Laval University)H-Index: 5
#2Ch. H. Detriche (INSA: Intelligence and National Security Alliance)H-Index: 5
Last. Michel Pigeon (Laval University)H-Index: 27
view all 3 authors...
La durabilite des reparations non armees en beton de ciment est souvent compromise par l'empechement du retrait du nouveau beton au contact de l'ouvrage repare, les contraintes dues au retrait contrarie au contact beton neuf-ancien, beton pouvant causer a terme le decollement de la reparation. Le fluage permet un certain relâchement des contraintes dues au retrait; il est egalement possible que l'ouverture d'un reseau dense et uniformement reparti de microfissures puisse permettre une relaxation...
1 CitationsSource
#1A. Bascoul (INSA: Intelligence and National Security Alliance)H-Index: 3
#2Ch. H. Detriche (INSA: Intelligence and National Security Alliance)H-Index: 5
Last. S. Ramoda (INSA: Intelligence and National Security Alliance)H-Index: 1
view all 3 authors...
La resistance a la propagation de fissures d'un materiau heterogene tel que le mortier ou le beton hydraulique est liee aux caracteristiques de la phase granulaire d'une part, a celles de la matrice et des aureoles de transition, d'autre part. Nous examinons plus particulierement ici le role des caracteristiques de la phase liante sur la resistance a la propagation de fissures des mortiers. Celle-ci est determinee en mode I en utilisant un essai de flexion trois points, controle en deplacement, ...
1 CitationsSource
#1Ch. H. Detriche (INSA: Intelligence and National Security Alliance)H-Index: 5
#2S. Ramoda (INSA: Intelligence and National Security Alliance)H-Index: 1
Dans un materiau heterogene tel que le mortier ou le beton de liant hydraulique, le comportement mecanique depend des differentes parties constitutives et de leur association. Nous examinons plus particulierement ici le role de la concentration en liant dans la matrice et des proportions relatives matrice-granulats sur les conditions de resistance des mortiers a la propagation des fissures. Celle-ci a ete determinee en Mode I en utilisant un essai de flexion trois points, controle en deplacement...